Pascal and Francis Bibliographic Databases

Help

Search results

Your search

kw.\*:("ACIERA CR:2-2,5 MO:0,5-1 C:0,03-0,1")

Publication Year[py]

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Discipline (document) [di]

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Language

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Author Country

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Origin

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Results 1 to 19 of 19

  • Page / 1
Export

Selection :

  • and

HIGH TEMPERATURE PROPERTIES OF 21/4 CR-1 MO WELD METAL = CARACTERISTIQUES A HAUTE TEMPERATURE DU METAL FONDU EN ACIER A 21/4 CR-1 MOLUNDIN CD; KRUSE BJ; PENDLEY MR et al.1982; WELD. RES. COUNC. BULL.; ISSN 0043-2326; USA; DA. 1982; NO 277; PP. 1-27; BIBL. 139 REF.; LOC. ISArticle

Effect of cold work on the oxidation resistance of 21/4 Cr-1 Mo steel = Influence du travail à froid sur la résistance à l'oxydation d'un acier Cr 21/4-Mo1KHANNA, A. S; GNANAMOORTHY, J. B.Oxidation of metals. 1985, Vol 23, Num 1-2, pp 17-33, issn 0030-770XArticle

DEVELOPMENT OF HOLLOW INGOT FOR LARGE FORGING = ENTWICKLUNG EINES HOHLBLOCKES FUER GROSSE SCHMIEDESTUECKE = MISE AU POINT D'UN LINGOT CREUX POUR DE GRANDES PIECES DE FORGEIIDA Y; YAMAMOTO T; YAMAURA S et al.1982; TRANS. IRON STEEL INST. JPN.; JPN; DA. 1982-05; VOL. 22; NO 5; PP. 333-341; BIBL. 6 REF.Article

Die Restlebensdauer von industriellen Hochtemperaturmaterialien = Life prediction of industrial high temperature materialsWALSER, B; ROSSELET, A.Material + technik. 1985, Vol 13, Num 1, pp 36-43, issn 0376-6845Article

Zkus = Experiences in maintenance and preparation for general repair of a reforming furnace for petrol productionSTROUKAL, V.Zváranie. 1983, Vol 32, Num 4, pp 113-117, issn 0044-5525Article

ROHRE AUS WARMFESTEN STAEHLEN KALTVERFORMT ZEIGEN VERAENDERUNG DES GEFUEGES = INFLUENCE OF COLD FORMING OF HOT STRENGTH STEEL TUBES ON THE STRUCTUREESMAIL NAD R; MACH K.1981; MM, MASCHINENMARKT; DEU; DA. 1981-09-04; VOL. 87; NO 70; PP. 1435-1438Article

Creep behaviour of 2.25Cr1Mo steel from a service-exposed headerRUI WU; SANDSTRÖM, R; STORESUND, J et al.Materials at high temperatures. 1992, Vol 10, Num 3, pp 164-170, issn 0960-3409Article

Through-thickness creep damage in a service-exposed header of 2.25Cr1Mo steelRUI WU; SANDSTRÖM, R; STORESUND, J et al.Materials at high temperatures. 1992, Vol 10, Num 3, pp 154-163, issn 0960-3409Article

Metoda odhadu dynamické lomové houz = Method of estimation of dynamic fracture toughness of weldable structural steelsVLACH, B; HOLZMANN, M; MAN, J et al.Zváranie. 1982, Vol 31, Num 8, pp 227-232, issn 0044-5525Article

TEMPERING OF 2.25 PCT CR-1 PCT MO LOW CARBON STEELS = REVENU DES ACIERS A BAS CARBONE 2,25% CR-1% MOPILLING J; RIDLEY N.1982; METALL. TRANS. A; ISSN 0360-2133; USA; DA. 1982; VOL. 13; NO 4; PP. 557-563; BIBL. 11 REF.Article

Schaelen dickwandiger Rohre in Produktionslinien = Peeling of thick-walled pipes in production linesLINDEMANN, W.Bänder, Bleche, Rohre. 1983, Vol 24, Num 12, pp 347-350, issn 0005-3848Article

Verfestigung von Staehlen bei kleinen Verformungsgraden und ihre Auswirkungen auf den Festigkeitskennwert. T. 1 = Strengthening of steels with low degrees of deformation and its effects on strength characteristics. Pt. 1KRAEGELOH, E.VGB Kraftwerkstechnik. 1985, Vol 65, Num 9, pp 858-868, issn 0372-5715Article

A STUDY OF STRESS RELIEF CRACKING IN 2 1/4 CR1MO STEEL. PT. 2:THE EFFECTS OF MULTI-COMPONENT SEGREGATIONHIPPSLEY CA; KNOTT JF; EDWARDS BC et al.1982; ACTA METALL.; USA; DA. 1982-03; VOL. 30; NO 3; PP. 641-654; BIBL. 40 REF.Article

OPTIMALER EINSATZ WARMFESTER ROHRSTAEHLE = OPTIMAL USE OF CREEP RESISTANT TUBE STEELSFISCHER K.1981; FREIBERG. FORSCHUNGSH., REIHE B; DDR; DA. 1981; VOL. 221; PP. 93-100; BIBL. 7 REF.Conference Paper

STRESS CORROSION CRACKING OF STEELS IN CO-CO2-H2O ENVIRONMENTSUEKADO M; SAKAI K; KIYOSHIGE M et al.1981; TETSU TO HAGANE; JPN; DA. 1981-07; VOL. 67; NO 9; PP. 1542-1550; BIBL. 12 REF.Article

Oxidation behaviour of 21/4 Cr-1Mo and 21/4 Cr-1Mo-Nb steels = Oxydation des aciers 21/4 Cr-1Mo et 21/4Cr-1Mo-NbKHANNA, A. S; GNANAMOORTHY, J. B; RODRIGUEZ, P et al.Transactions of the Indian Institute of Metals. 1987, Vol 40, Num 6, pp 503-513, issn 0019-493XArticle

Stress-driven solute enrichment of crack-tips during low-ductility intergranular fracture of low-alloy steel = Spannungsgetriebene Anreicherung geloester Atome an Rissspitzen waehrend des niederduktilen intergranularen Bruches in niedriglegiertem StahlHIPPSLEY, C.A; RAUH, H; BULLOUGH, R et al.Acta metallurgica. 1984, Vol 32, Num 9, pp 1381-1394, issn 0001-6160Article

Rauchgasseitige Hochtemperaturkorrosion und Versproedung von Ueberhitzerrohren aus X 20 CrMoV 12 1 = Combustion gas side high temperature corrosion and embrittlement of superheated tubes made of X 20 CrMoV 12 1EFFERTZ, P.H; WOITSCHECK, A.1987, Vol 60, Num 3, pp 113-120, issn 0025-4517Article

Technologie der Waermebehandlung warm- und hochwarmfester Staehle = Heat treatment for hot-strength steelsBRANDIS, H; HUCHTEMANN, B; STEINEN, A. von den et al.1985, Vol 79, Num 4, pp 9-12, issn 0039-8667Article

  • Page / 1